This is PETG, one was left out in about 40% humidity the other was dried to about 20%

    • the16bitgamer@programming.devOP
      link
      fedilink
      English
      arrow-up
      3
      ·
      10 days ago

      It’s PETG and I’ve moved to a very wet environment. Stringing and popping and a big issue here. My last place though was a lot dryer and didn’t need this solution.